Heat Setting Workshop

TTK Heat Setting Workshop runs 3 Monforts stenters and a 31-chamber oven, focused on low-tension heat setting. We handle stenter setting, after-setting, heat setting and setting of customer-supplied fabric.

Standardized production workshop · Continuous line of the heat-setting section

Introduction

Heat setting is a physical finishing process. Once a fabric has been coated or laminated, the temperature window of the coating and film, the softening point of the hot-melt adhesive and the elastic recovery of the base fabric together determine the temperature and tension this step can use. We set the process from the incoming material system rather than running every fabric on one set of parameters.

The equipment is built around low-tension setting and handles knitted, woven and stretch fabrics. For stretch fabric the question is how much elastic recovery is retained; for high-density woven fabric it is whether the width holds. When tension is too high, these are the first two to fail.

Heating is by steam: stable temperature and even heat, avoiding the hardening and shade change caused by local overheating. The line has oil-free rails and a photoelectric weft straightener — the former lowers the risk of oil marks on the fabric, the latter detects weft skew online and reduces the variation of manual correction.

Besides setting itself, the workshop also has a rotary-spray single-side machine for single-side repellent / single-side absorbent finishing, and it can top up water repellency after lamination or coating. We take both setting and functional finishing of customer-supplied fabric, and setting alone can also be ordered as a single process.

Equipment Configuration

——
Stenters3 × Monforts stenters, each with independent chamber temperature control
Oven chambers1 × 11 chambers + 2 × 10 chambers, 31 chambers in total
Max. width175 cm
Capacity per stenter50,000–80,000 m/day
Total capacityapprox. 150,000–240,000 m/day, varying by article
Accepted incoming fabricFabric already finished with PU, PA, solvent-free PU/PUR or PVC coating, plus laminated and printed fabric
Order modeFull order or single process

Process Flow

Indicative, not to scale; maximum working width 175 cm

  1. 01Incoming inspectionWidth, weight, skew, coating or lamination state
  2. 02Low-tension settingTemperature, tension and speed set from the incoming system; knitted, woven and stretch fabrics
  3. 03Dryer, 31 chambers3 × Monforts stenters, each with independent chamber temperature control
  4. 04Visual inspectionWidth, skew and appearance checked; samples retained

Equipment & process

Steam heating

Stable temperature, even heat; less hardening and shade change from local overheating

Oil-free rail

Lower risk of oil marks on the fabric

Photoelectric weft straightener

Detects skew online and reduces the variation of manual correction

Pin plate calibration

Pins arranged and calibrated; hard pin marks and pin bars are less likely

Key Data

15–24m/day Total capacityVaries by article
±0.5cm Width toleranceMeasured online and recorded every 300 yards
≤±1.0% Warp and weft shrinkageInternal standard; reported figure follows the test report
100washes Antibacterial wash durabilityPer the workshop's process documents
500m Minimum orderBelow 500 m, use the sampling route
1–5days Standard lead timeLonger for multi-step combinations
1day SamplingSample and test data the next day
27finishes Functional FinishesThree-proof, moisture wicking, UV protection, flame retardant and more

Precision Control

Width

Maximum working width 175 cm, tolerance within ±0.5 cm; measured online and recorded every 300 yards.

Shrinkage

Internal standard is ≤±1.0% warp and weft; the reported figure follows the corresponding test report.

Weft skew

A photoelectric skew corrector detects and corrects online; the exit is also checked visually to reduce the variation of manual correction.

27 functional finishes

Water-repellent routes: both fluorine-free (C0) and fluorinated C6/C8 are available, selected per customer requirement and restricted-substance list.

Certifications & Testing

Certifications (11 items)

Testing

Testing is handled by the TTK Test Centre. It is our in-house laboratory, covering in-process and final inspection with a testing view independent of the production line; when an external institution's report is needed, we can arrange submission and help verify it.

Sampling & Delivery

  1. Sampling in 1 dayScheduled the same day once the process is confirmed; sample and test data the next day
  2. 500 mMinimum order;Below 500 m, use the sampling route
  3. 1–5 daysStandard lead time;Longer for multi-step combinations

Sampling, minimum order and lead time are all confirmed on the order, with peak-season dates against the confirmed sheet.

Request a Sample →

FAQ

Q1Which fabrics suit low-tension heat-setting?

Knitted, woven and stretch fabrics, with or without elastane. Low tension suits stretch-sensitive fabric: it is how elastic recovery and hand feel are kept.

Q2Why steam heating?

Steam keeps the temperature stable and heats the fabric evenly, so local overheating does not harden the fabric or change its shade.

Q3What do oil-free rails solve?

They lower the risk of oil marks. Rails that need lubrication leave marks on light shades and on high-end orders; oil-free rails remove that source at the machine.

Q4Will the pins leave pin marks or pin bars?

The pins are arranged and calibrated, so hard pin marks and pin bars are less likely, and the selvedge stays neat.

Q5How is skew controlled?

A photoelectric skew corrector detects and corrects online, with a visual check at the exit, reducing the variation of manual correction.

Q6What stenters do you run?

Three Monforts lines: 11 dryer chambers on one, 10 on each of the other two, 31 in total, each with independently controlled sections.

Q7How is the setting temperature decided?

From the temperature limits of the fibre and the finishing agents, not as a fixed value. Polyester usually sets at 180–190 °C; coated and laminated fabric is set lower, within the coating and agent limits, so neither is damaged.

Q8How do PU, PA and solvent-free PU coatings differ in setting?

Their temperature limits set the range. PA takes a higher range for full setting; PU needs a capped temperature to protect the micro-phase structure and hand feel; solvent-free PU balances cure and setting.

Q9Can you set incoming fabric that already has a PVC coating?

Yes; we process the finished PVC-coated fabric as incoming material. PVC-coated fabric is usually made by calendering at around 160–185 °C, so it enters setting at a low temperature to prevent plasticiser migration, tackiness and shrinkage. The exact temperature follows the incoming state, set at process review.

Q10Will setting delaminate laminated fabric?

When temperature matches the adhesive's softening point and tension stays low, the laminate holds. Coating cracking and separation come from too high a temperature or too much tension.

Q11What is the maximum width and tolerance?

Maximum working width 175 cm; normal widths are set per order, with tolerance within ±0.5 cm.

Q12What is the capacity?

Three stenters at 50,000–80,000 m/day each, about 150,000–240,000 m/day in total; actual capacity varies with article, width and process complexity.

Q13Which functional finishes do you offer?

27: three-proof, fluorine-free (C0) water repellency, single-side repellency and absorbency, antibacterial, anti-mould, flame retardant, UV protection, far infrared, cool touch, moisture wicking, fragrance, anti-wrinkle, anti-static, easy-clean, anti-pilling, down-proof, windproof, water repellent, hydrophilic, oil repellent, anti-mite, insect repellent, mothproof, negative ion, thermal / heat storage, vitamin A skin care and collagen skin care.

Q14Can water repellency lost in finishing be restored?

Sampling first. The rotary-spray machine tops up repellency by controlled spraying and brings part of it back; whether it applies depends on the fabric state and the following processes.

Q15What does "single-side repellent, single-side absorbent" mean?

Water repellent on one face, hydrophilic on the other: the face repels, the back absorbs, common in sportswear and outdoor fabric for one-way moisture transport.

Q16What else can the spray machine do?

It raises peel strength on laminated fabric and supports combinations such as repellency after lamination or after coating.

Q17How many washes does the antibacterial finish take?

Per the workshop's process documents, 100 washes.

Q18What is the difference between fluorine-free and fluorinated water repellency?

We run both routes: fluorine-free (C0) and fluorinated C6/C8. The choice follows the customer's requirement, end use and restricted-substance list; specific substances follow the customer's RSL and test reports.

Q19What are microcapsule finishes?

Functional substances encapsulated and released slowly for longer effect, such as microcapsule heat storage, fragrance and cool-touch microcapsules.

Q20What width tolerance can you hold?

Normally within ±0.5 cm, measured online and recorded every 300 yards; tighter requirements can be agreed at process review.

Q21What shrinkage can you hold?

Internal target is ≤±1.0% warp and weft; the reported figure follows the corresponding test report.

Q22How are oil marks or pin marks traced?

Oil-free rails and calibrated pins reduce both at the machine, and the process is recorded end to end so a defect can be traced to coating, lamination or setting.

Q23Which management-system certifications do you hold, and who does the testing?

Certifications (11 items, names only): ISO 9001, ISO 14001, ISO 45001, GJB 9001C-2017, GRS, RCS, OEKO-TEX® STANDARD 100, HIGG FEM, HIGG FSLM, RWS; also a bluesign® SYSTEM PARTNER. Testing is handled by the TTK Test Centre, our in-house laboratory, for in-process and final inspection; when an external institution's report is needed, we can arrange submission and help verify it.

Q24Do you take outside material?

Yes, for setting and functional finishing. Incoming material is inspected first to confirm it suits setting.

Q25How are sampling, minimum order and lead time set?

Sampling in 1 day: scheduled the same day after the process is confirmed, with sample and test data the next day. Minimum order 500 m; below that, use the sampling route. Standard lead time 1–5 days, longer for multi-step coating and lamination combinations. Sampling, minimum order and lead time are all confirmed on the order, with peak-season dates against the confirmed sheet.